Presentation is loading. Please wait.

Ni-W Liquid Phase Sintering T A B A powder + B powder L T sint A+B.

Similar presentations


Presentation on theme: "Ni-W Liquid Phase Sintering T A B A powder + B powder L T sint A+B."— Presentation transcript:

1 Ni-W Liquid Phase Sintering T A B A powder + B powder L T sint A+B

2 LPS as flow through packed beds- the chemical engineering approach The space between particles-the interconnected porosity-are pipes. These pipes have an effective radius (hydraulic radius) given as 2r a 2R

3 2r a 2R Example 2R2R

4 Example (continued) Now determine the hydraulic radius

5 Example (continued) See Gaskell 2.6 and the Die Cast Mold Filling Example

6 Example (continued)

7 Liquid Polycrystalline particle Grain boundary ‘wetting’ breaks the polycrystalline particle into single crystal particles in the initial stages of liquid phase sintering. These single crystal particles then spheroidize and coarsen.

8 Youngs’ Equation Represent the surface tensions of a multi-phase junction as vectors drawn parallel to the respective surfaces The surface energies for the for the solid/liquid, the solid/vapor and the liquid/vapor interfaces are γ sl, γ sv, γ lv. The vectors representing these surface energies must balance at the three phase triple junction. This equation representing this balance is known as ‘Youngs’ equation” γ sl γ sv γ lv θ

9 γ sl γ sv γ lv θ γ sl γ sv γ lv θ Large γ sl, non-wetting θ Large Large γ sv, wetting θ small

10 Grain A Grain B Liquid γ BL γ AL γ AB θBθB θAθA Grain boundary wetting during LPS occurs when θ A and θ B approach zero.