Chapter 7: Dislocation and Strengthening Mechanism

Similar presentations


Presentation on theme: "Chapter 7: Dislocation and Strengthening Mechanism"— Presentation transcript:

1 Chapter 7: Dislocation and Strengthening Mechanism
Why Study ? With a knowledge of the nature of dislocation and the role they play in the plastic deformation process, we are able to understand the underlying mechanisms of the techniques that are used to strengthen and harden metals and alloys.

2 DISLOCATIONS and PLASTIC DEFORMATION 7.2 Basic Concepts
Dislocation Types Edge Dislocation Screw Dislocation Review from Chapter 4 notes

3 Chapter 4 (Review) 4.4 Dislocations __ Linear Defects
A dislocation is a linear or one-dimensional defect around which some of the atoms are misaligned. Edge dislocation: An extra portion of a plane of atoms, or half-plane, the edge of which terminates within the crystal. (shown in figure ) Dislocation line: For the edge dislocation in Figure, it is perpendicular to the plane of the paper.

4 Chapter 4 (Review) 4.4 Dislocations __ Linear Defects (Contd.)
Within the region around the dislocation line, there is some localized lattice distortion. Atoms above the line are squeezed together Those below are pulled apart Results in slight curvature for the vertical planes of atoms as they bend around this extra-half plane At far position, the lattice is virtually perfect.  extra half-plane in the upper portion extra half-plane in the bottom portion

5 Chapter 4 (Review) 4.4 Dislocations __ Linear Defects
Screw Dislocation : May be thought of as being formed by a shear stress that is applied to produce the distortion as shown in figure. The upper front region of the crystal is shifted one atomic distance to the right relation to the bottom portion. Atomic distortion is also linear and along a dislocation line, Line AB. Derived name from the spiral or helical path or ramp traced around the dislocation line.  Symbol in Figure

6 Chapter 4 (Review) 4.4 Dislocations __ Linear Defects
Most dislocations found in crystalline materials are probably neither pure edge nor pure screw, but mixed. All three dislocations are represented in Figure 4.5 The lattice distortion that is produced away from the two faces is mixed, having varying degrees of screw and edge character.

7 Plastic deformation corresponds to the motion of large number of dislocations.
An edge dislocation moves in response to a shear stress applied in a direction perpendicular to its line Figure shows the mechanics.

8 When the shear stress applied,
Plane A is forced to the right This in turn pushes the top halves of planes B, C, D, and so on. If the applied stress is of sufficient magnitude, The inter-atomic bonds of plane B are severed along the shear plane The upper half of plane B becomes the extra half-plane Plane A links up with the bottom half-plane of plane B This process is subsequently repeated Ultimately this extra half-plane may emerge  forming an edge that is one atomic distance wide Atomic arrangement of the crystal Only during passage of the extra half-plane the lattice structure is disrupted Before and after the movement of a dislocation  ordered and perfect

9 SLIP  The process by which plastic deformation is produced by dislocation
Slip plane  the crystallographic plane along which the dislocation line traverses Macroscopic plastic deformation simply corresponds to permanent deformation that results from the movement of dislocations, or slip, in response to an applied shear stress The direction of movement for For an edge is parallel to the applied shear stress For Screw dislocation is perpendicular Net plastic deformation for both is same

10 IBCAST: Introduction to Nonlinear FEA
14th June, 2002. Dislocation Motion Dislocation moves along slip plane in slip direction perpendicular to dislocation line Slip direction same direction as Burgers vector Edge dislocation Adapted from Fig. 7.2, Callister 7e. Screw dislocation By: Dr. A.F.M. Arif

11 Dislocation motion is analogous to the mode of locomotion employed by a caterpillar
Forms hump near its posterior end by pulling last pair of legs a unit leg distance  hump propelled forward by repeated lifting and shifting  when hump reached the anterior end, the entire caterpillar has moved forward by the leg separation distance.

12 Some dislocations in all crystalline materials were introduced during
Solidification Plastic deformation Thermal stresses Dislocation density expressed as Total dislocation length per unit volume, or equivalently (mm/mm3) The number of dislocations that intersect a unit area of a random section (mm-2) Carefully solidified crystals have low values: 103 mm-2 Heavily deformed metal have high values: 109 to 1010 mm-2 Heat treating a deformed metal diminishes to: 105 to 106 mm-2

13 7.3 Characteristics of Dislocations
When metals are deformed plastically, Some fraction of the deformation energy (approx. 5%) is retained internally Remainder is dissipated as heat Major portion of stored energy is as strain energy associated with dislocations. Lattice distortions may be considered to be strain fields That radiate from the dislocation line Extend into the surrounding atoms Magnitude decreases with radial distance from the dislocation.

14 Atoms immediately above and adjacent to the dislocation line  squeezed together  experiencing compressive strain Atoms directly below  tensile strain Shear strain also exist in the vicinity of edge dislocation For screw dislocation, lattice strains are pure shear only

15 Strain fields surrounding dislocations in close proximity may interact
Examples Two edge dislocations having same sign and identical slip plane Compressive and tensile strain field for both lie on the same side of the slip plane Strain field interaction  mutual repulsive force that tends to move them apart.

16 Two dislocations of opposite sign and having the same slip plane
Attract each other Dislocation annihilation will occur when they meet Two extra half-planes align and become a complete plane Are possible between edge, screw, and/or mixed dislocations Result in strengthening mechanism for metals.

17 7.4 Slip Systems Dislocations produce atomic dislocations on specific crystallographic slip planes and in specific crystallographic slip directions. Slip is favored on close-packed planes since a lower shear stress for atomic displacement is required than for less densely packed planes  Plane having greatest planar density  Slip Plane If slip on the closed-packed planes is restricted due to local high stresses, for example, then planes of lower atomic packing can become operative Slip in the closed-packed directions is also favored since less energy is required to move the atoms from one position to another if the atoms are closer together  Directions having highest linear density  Slip Direction A combination of a slip plane and a slip direction is known as Slip System.

18 Slip System

19 Deformation Mechanisms
IBCAST: Introduction to Nonlinear FEA 14th June, 2002. Deformation Mechanisms Slip System Slip plane - plane allowing easiest slippage Wide interplanar spacings - highest planar densities Slip direction - direction of movement - Highest linear densities FCC Slip occurs on {111} planes (close-packed) in <110> directions (close-packed) => total of 12 slip systems in FCC in BCC & HCP other slip systems occur Adapted from Fig. 7.6, Callister 7e. By: Dr. A.F.M. Arif

20 For metals with FCC structure, slip takes place
On the close-packed octahedral planes: In the closed-packed directions: There are eight {111} octahedral planes which are crystallographically equivalent  same planar density Planes at opposite faces, which are parallel, are considered the same type of (111) slip plane Therefore, there are only four different types of (111) slip planes in the FCC crystal structure Each (111)-type plane contains three directions, which are crystallographically equivalent. Reverse directions are not considered different slip directions Thus, for FCC lattice structure 4 unique slip planes x 3 independent slip directions = 12 slip systems

21

22

23

24 Possible slip systems for BCC and HCP are listed in Table 7.1
Metals with FCC or BCC crystal structures have a relatively large number of slip systems (at least 12) These metals are quite ductile because plastic deformation is normally possible along the various systems HCP metals having few active slip systems are normally quite brittle.

25 7.5 Slip in Single Crystal Edge, Screw, and mixed dislocations move in response to shear stresses applied along a slip plane and in a slip direction. Even for applied pure normal (tensile or compressive) stress, shear stress exists at all but parallel or perpendicular alignments to the applied stress direction.  resolved shear direction Magnitude of resolved shear stress: A metal single crystal has a number of different slip systems Resolved shear stress normally differs for each one

26 STRESS AND DISLOCATION MOTION
• Crystals slip due to a resolved shear stress, tR. • Applied tension can produce such a stress. slip plane normal, ns direction slip direction slip direction slip 4

27 Critical resolved stress ( tcrss )
Minimum shear stress required to initiate slip Property of material that determines when yielding occurs

28 CRITICAL RESOLVED SHEAR STRESS
• Condition for dislocation motion: • Crystal orientation can make it easy or hard to move disl. 5

29 IBCAST: Introduction to Nonlinear FEA
14th June, 2002. Single Crystal Slip Slip occurs along a number of equivalent and most favorably oriented planes and directions at various positions along the length. On surface these appears as lines (Figure 7.9) Adapted from Fig. 7.9, Callister 7e. Adapted from Fig. 7.8, Callister 7e. By: Dr. A.F.M. Arif

30 Example 7.1

31 Ex: Deformation of single crystal
IBCAST: Introduction to Nonlinear FEA 14th June, 2002. Ex: Deformation of single crystal a) Will the single crystal yield? b) If not, what stress is needed? =60° crss = 3000 psi =35° Adapted from Fig. 7.7, Callister 7e.  = 6500 psi So the applied stress of 6500 psi will not cause the crystal to yield. By: Dr. A.F.M. Arif

32 Ex: Deformation of single crystal
IBCAST: Introduction to Nonlinear FEA 14th June, 2002. Ex: Deformation of single crystal What stress is necessary (i.e., what is the yield stress, sy)? So for deformation to occur the applied stress must be greater than or equal to the yield stress By: Dr. A.F.M. Arif

33 7.6 Plastic Deformation of Polycrystalline Materials
Random crystallographic orientations of the numerous grains, the direction of slip varies from one grain to another  deformation and slip is complex Photomicrograph of a polycrystalline copper specimen Before deformation, the surface was polished Slip lines visible Two sets of parallel yet intersecting sets of lines  It appears that two slip systems operated The difference in alignment of the slip lines for the several grains  variation in grain orientation

34 Gross plastic deformation  distortion of individual grain by means of slip
Mechanical integrity and coherency are maintained  grain boundaries usually do not come apart or open up. Each individual grain is constrained by its neighboring grains. Figure 7.11 shows plastic deformation Before deformation, grains equiaxed (have approx. same dimension in all direction) After deformation, grains elongated along the direction of extension or loading

35 Polycrystalline materials are stronger
greater stresses are required to initiate slip and yielding Due to geometrical constraints imposed on the grains Even a favorably oriented single grain can not deform until the adjacent less favorably oriented grains are capable of slip also  requires a higher applied stress level.

36 Mechanism of Strengthening in Metals
The ability of a metal to plastically deform depends on the ability of dislocations to move. Hardness and strength are related to the ease with which plastic deformation can be made to occur To enhance mechanical strength  reduce dislocation mobility  greater mechanical forces required to initiate plastic deformation. Strengthening mechanism for single phase metal By grain size reduction Solid-solution alloying Strain-hardening

37 7.8 Strengthening by Grain Size Reduction
Adjacent grains have different crystallographic orientation During plastic deformation, slip or dislocation motion must take place across the common boundary (from grain A to grain B) Grain boundary acts as a barrier to dislocation motion for two reasons: Two grains are of different orientation  a dislocation have to change its direction of motion  becomes more difficult as crystallographic misorientation increases. Atomic disorder within a grain boundary region will result in a discontinuity of slip planes from one grain into the other.

38 Hall-Petch Equation: For many materials, Yield strength varies with grain size as
d: average grain diameter s0 and ky are material constants Figure 7.15 shows strength variation for brass Hall-Petch equation is not valid for very large and extremely small grain materials

39

40 High-angle grain boundaries
Dislocations may not traverse grain boundaries during deformation A stress concentration ahead of a slip plane in one grain may activate sources of new dislocation in an adjacent grain. Small-angle grain boundaries Not effective in interfering because of slight misalignment Twin boundaries Effectively block slip and increase the strength of the material Boundaries between two different phases Impediment (obstacle/barrier) to movements of dislocations Important in strengthening complex alloys

41 7.9 Solid Solution Strengthening
Another technique to strengthen and harden metals is alloying Adding impurity atoms that go into either substitutional or interstitial solid solution High-purity metals are almost always softer and weaker Fig 7.16 shows the effect of alloying nickel in copper

42

43 Alloys are stronger than pure metals
Impurity atoms impose lattice strain on surrounding host atoms Lattice strain field interaction between dislocation and impurity atoms result  dislocation movement is restricted An impurity atom that is smaller than a host atom  substitution results tensile strains on the surrounding crystal lattice ( Fig 7.17a) Larger substitutional atom imposes compressive strains in its vacinity (Fig 7.18a)

44

45 Solute atoms tend to diffuse to and segregate around dislocations  reduce strain energy  to cancel some lattice strain surrounding a dislocation To accomplish this, a smaller impurity atom is located where its tensile strain will partially nullify some of the dislocation’s compressive strain A larger atom to nullify tensile strain of dislocation  Figure 7.17b and 7.18b Resistance to slip is greater Overall lattice strain must increase if dislocation is torn away from them Same strain interaction exist between atoms and dislocation that are in motion during plastic deformation  greater applied stress is needed to initiate and continue plastic deformation

46 7.10 Strain Hardening Strain hardening  a phenomenon whereby a ductile material becomes harded and stronger as it is plastically deformed. Also known as work-hardening or cold working Most metals strain harden at room temperature Degree of plastic deformation is expressed as percent cold work (%CW)

47 Figure demonstrates effect of cold work on steel, brass and copper
Loading to plastic deformation, unloading and then reloading  requires more applied load or stress to yield  metal becomes stronger

48 Why more stronger ? On the average, dislocation-dislocation strain interactions are repulsive Dislocation density increases due to Deformation or cold work Dislocation multiplication Formation of new dislocations Net result  motion of dislocation is hindered by the presence of other dislocations  higher imposed stress is needed to deform a metal

49 Recovery, Recrystallization, and Grain Growth
Plastic deformation of polycrystalline metal at temperatures lower than its melting temperature produces  micro-structural and property changes  includes A change in grain shape Strain hardening Increase in dislocation density Some fraction of deformation energy (about 5%) stored in metal as strain energy Associated with tensile, compressive and shear zones around newly created dislocations Other properties (such as electrical conductivity and corrosion resistance ) may be modified by plastic deformation.

50 Modified Properties and structures due to plastic deformation (cold work)
May revert back to the precold-worked states by Annealing Annealing is a heat treatment process Restoration due to due different processes at elevated temperatures Recovery Recrystallization Above processes may be followed by grain growth.

51 7.11 Recovery At elevated temperature  enhanced atomic diffusion  dislocation motion  some stored strain energy relieved Recovery process Involves Reduction in dislocation numbers Dislocation configuration with low strain energy (similar to Fig 4.8) Physical properties are recovered to their precold-worked state Electrical and thermal conductivities

52 7.12 Recrystallization Even after recovery is complete, the grains are still in a relatively high strain energy state. Recrystallization is the formation of a new set of strain-free and equiaxed grains having low dislocation densities as the precold-worked state. Difference in internal energy between the strained and unstrained material  acts as the driving force to produce new grain structure New grains form as very small nuclei  grow until completely replace the parent material  involves short-range diffusion

53 7.12 Recrystallization (Contd.) Several stages of recrystallization
(a) cold-worked (33%) grain structure (b) Initial stage of recrystallization after heating 3 s at 580oC

54 7.12 Recrystallization (Contd.) Several stages of recrystallization
(c) Partial replacement of cold-worked grains by recrystallized ones (4s at 580oC) (d) complete recrystallization (8s at 580oC)

55 7.12 Recrystallization (Contd.) Several stages of recrystallization
(e) Grain growth after 15 min at 580oC (d) Grain growth after 10 min at 700oC

56 7.12 Recrystallization During recrystallization, mechanical properties restored to their precold-worked values Metal becomes softer, weaker, yet ductile Some heat treatments are designed to allow recrystallization to occur these modifications in the mechanical characteristics. Recrystallization depends on both time and temperature Influence of time The degree (or fraction ) of recrystallization increases with time (Figure 7.21a-d)

57 Influence of temperature
Figure 7.22 shows tensile strength and ductility of a brass alloy Constant heat treatment time of 1 hour Grain structures at various stages are presented schematically.

58 Recrystallization temperature
The temperature at which recrystallization just reaches completion in 1 hour. Recrystallization temperature of brass alloy (Fig 7.22) is about 450oC (850oF). It is about 1/3 to ½ of absolute melting temperature Depends on several factors, such as % cold work, purity of alloy etc. Effect of %CW Increasing %CW enhances the rate of recrystallization  recrystallization temperature is lowered Recrysttalization temperature approaches a constant or limiting value at high deformation. Critical degree of cold work Below which no recrystallization Ususally 2 – 20 %

59

60 Effect of alloying Recrystallization proceeds more rapidly in pure metal than in alloys  alloying raises recrystallization temperature For pure metal: normally it is 0.3(Melting temperature) For alloys, it may run as high as 0.7(melting temperature) Hot working : plastic deformation operations at temperatures above the recrystallization temperature Material remains relatively soft and ductile during deformation It does not strain harden Large deformations possible

61 Design Example 7.1

62 7.13 Grain growth After recrystallization is complete, the strain-free grains will continue to grow if the metal specimen is left at the elevated temperature  phenomenon is known as grain growth. It occurs by the migration of grain boundaries Boundary motion is just the short-range diffusion of atoms from one side of the boundary to the other Direction of boundary movement and atomic motion are opposite. Schematic reprsentationin Fig 7.24

63 For many polycrystalline materials, grain diameter (d) varies with time as
dn – don = Kt do : initial grain diameter at t=0 K, n: time-dependent constants n is equal to greater than 2 Dependence of grain size on time and temperature is shown in Fig 7.25 Brass alloy At higher temperature, rapid growth  due to enhancement of diffusion rate

64

65 Mechanical properties at room temperature of a fine-grained metal are usually superior (strength and toughness) than coarse-grained ones. If grain structure of a single phase alloy is coarser than that desired  plastically deform  subject to recrystallization heat treatment  refine grain size


Download ppt "Chapter 7: Dislocation and Strengthening Mechanism"

Similar presentations


Ads by Google