Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser.

Similar presentations


Presentation on theme: "Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser."— Presentation transcript:

1 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 Vibration plate dimension (mm) and instrumentation locations Figure Legend:

2 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 Vibratory analysis of the chordwise mode on a square plate: (a) von Mises stress and (b) mode shape Figure Legend:

3 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 Dogbone cutout orientation is used to separate the multiple sentences Figure Legend:

4 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 (a) DMLS build direction schematic and (b) top view of build structure Figure Legend:

5 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 Point cloud mesh to CAD geometry comparison: (a) cold-rolled and (b) specimen #7 DMLS before milling Figure Legend:

6 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 Forced response strain amplitude versus shaker head acceleration during sweeps: specimen #7 Figure Legend:

7 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 Forced response quality factor versus shaker head acceleration during sweeps: specimen #7 Figure Legend:

8 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 Ti 6Al–4V vibration bending fatigue life comparison Figure Legend:

9 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 Comparison of ultimate tensile strength deviation from population per fatigue plate Figure Legend:

10 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 Fractograph of DMLS specimen #1 Figure Legend:

11 Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2):022101-022101-7. doi:10.1115/1.4031271 SEM micrographs of Ti 6Al–4V: (a) DMLS and (b) cold-rolled Figure Legend:


Download ppt "Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser."

Similar presentations


Ads by Google